Tin Specification ASTM-B-545-97e1
Tin Plating Specification: ASTM-B-545-97e1
| Spec. | Thickness | Comment |
| ASTM-B- 545-97e1 |
ASTM requires purchaser to supply information, such as base metal, underplating, test requirements and test methods etc. In general, copper alloys containing more than 5% Zn shall have a copper undercoating of at least 0.0001" or nickel undercoating of at least 0.000050". | |
| Class A | .0001" min | |
| Class B | .0002" min | |
| Class C | .00032" min | .0004" min. for steel. |
| Class D | .0006" min | .0008" min. for steel. |
| Class E | .0012" min | ASTM requires purchaser to supply information, such as base metal, underplating, test requirements and test methods etc. In general, copper alloys containing more than 5% Zn shall have a copper undercoating of at least 0.0001" or nickel undercoating of at least 0.000050". |
| Type Matte | ||
| Type Bright | ||
| Type Flow- brightened |
----------- | Flow brightening available |